Notice: Function _load_textdomain_just_in_time was called incorrectly. Translation loading for the woo-discount-rules domain was triggered too early. This is usually an indicator for some code in the plugin or theme running too early. Translations should be loaded at the init action or later. Please see Debugging in WordPress for more information. (This message was added in version 6.7.0.) in /sites/esquell.wiljeonline.dev/files/web/wp/wp-includes/functions.php on line 6260
Co-firing of jewelry parts in metal clay - Esquell.eu

Co-firing of jewelry parts in metal clay

Co-firing of jewelry parts in silver clay, metal clay, silver clay / Art Clay Silver

925 and 999 silver are suitable for co-firing with silver clay.

In addition, there are stainless steel, bronze and copper haberdasheries suitable for co-firing with other types of metal clay.

Notice:

When co-firing 925 ( sterling) silver with silver clay, do not fire higher than 750 degrees Fahrenheit. At higher temperatures, sterling silver becomes brittle.

Notice:

Haberdashery and parts subject to tension, such as the back of earrings or the movable parts of the brooch, cannot be baked in because they lose their tension.

Available jewelry parts for co-baking

  • Screw eyes
  • Ear studs
  • Reverse spinning
  • Brooch Pins
  • Put trays
  • Settlements / chatons
  • Pendant eyes
  • 999 silver wire
  • Etc

Art Clay Silver Overlay paste

With Overlay paste from Art Clay Silver, firmly connect silver parts to your silver clay jewelry.